Carbon | 0.25% max | Phosphorous | 0.04% max |
Manganese | 1.60% max | Sulphur | 0.05% max |
Silicon | 0.50% max |
As a hot formed non admixture steel the capital characterisitics of S275 are its automated properties, such as the compactness backbone and crop strength.
Tensile Strength N/mm² (MPa) |
Yield Strength N/mm² (MPa) |
---|---|
380-540 | 275 |
(*as formed – 16mm plate)
With our material,we provide mill test certificate and ultrasonic Ok certificate (Note: Provide only if mentioned before placing the order.)